MEMSnet Home: MEMS-Talk: deposit stainless steel
deposit stainless steel
2003-03-26
Hongjun Zeng
2003-03-28
RobDavis
deposit stainless steel
Hongjun Zeng
2003-03-26
Dear all,

Anybody knows, or has the experience of depositing stainless steel on glass
or other insulating substrate?

Thanks,
Hongjun Zeng
Microfabrication Applications Laboratory (MAL)
University of Illinois at Chicago
ERF Building, 842 W. Taylor Street
Chicago, IL 60607-7022
Room 3014 ERF
Tel.: 312-413-5889, Fax: 312-996-6465



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation