MEMSnet Home: MEMS-Talk: Removing PDMS from SIO2
Removing PDMS from SIO2
2007-04-04
Petru Lunca Popa
2007-04-04
Xiaoguang "Leo" Liu
2007-04-04
Petru Lunca Popa
2007-04-04
Xiaoguang "Leo" Liu
Removing PDMS from SIO2
Petru Lunca Popa
2007-04-04
Thanks a lot. I will try and I will tell you what happened. I have to
be careful do not remove the gold from my Si

On 4/4/07, Xiaoguang Leo Liu  wrote:
> Hi Petru
>
> PDMS is pretty hard to remove once "hard" bonded to SiO2. You can try
> to use a blade or your tweezers to rip off the majority of the PDMS
> and try HCL:HNO3 3:1 to remove the residual. It worked for me once.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation