A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Removing PDMS from SIO2
Removing PDMS from SIO2
2007-04-04
Petru Lunca Popa
2007-04-04
Xiaoguang "Leo" Liu
2007-04-04
Petru Lunca Popa
2007-04-04
Xiaoguang "Leo" Liu
Removing PDMS from SIO2
Xiaoguang "Leo" Liu
2007-04-04
Hi Petru
I didn't know you had Au on your wafer. I think the HCL:HNO3 will
remove attach Au....
Best
Leo

On 4/4/07, Petru Lunca Popa  wrote:
> Thanks a lot. I will try and I will tell you what happened. I have to
> be careful do not remove the gold from my Si
>
> On 4/4/07, Xiaoguang Leo Liu  wrote:
> > Hi Petru
> >
> > PDMS is pretty hard to remove once "hard" bonded to SiO2. You can try
> > to use a blade or your tweezers to rip off the majority of the PDMS
> > and try HCL:HNO3 3:1 to remove the residual. It worked for me once.

--
Xiaoguang "Leo" Liu
Electrical and Computer Engineering
Purdue University
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing