MEMSnet Home: MEMS-Talk: Question on PDMS micro channels
Question on PDMS micro channels
2007-06-17
King Lai
2007-06-18
Gwennou Coupier
2007-06-18
Petru Lunca Popa
2007-06-18
Chris Bliss
2007-06-18
Joseph Grogan
Question on PDMS micro channels
Gwennou Coupier
2007-06-18
It is well known that alcohol can diffuse into PDMS and make it
inflate. Therefore it is a bad idea. Maybe other people have more
experience than me on that subject.

On Sun, 17 Jun 2007 18:18:50 +0800
  "King Lai"  wrote:
> Hi all,
>
> I am planning to make micro channels and chambers by PDMS, but
> acetone/alcohol will flow inside the micro channels. I would like to
>know if
> acetone and alcohol attack PDMS channel. Did anybody has experience
>in using
> acetone in PDMS channel?

Gwennou Coupier
Laboratoire de Spectrométrie Physique
Université Joseph Fourier
140, rue de la physique, 38402 St Martin d'Hères Cedex, France
Tel : 04 76 51 47 60
[email protected]
www.coupier.eu
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation