MEMSnet Home: MEMS-Talk: Question on PDMS micro channels
Question on PDMS micro channels
2007-06-17
King Lai
2007-06-18
Gwennou Coupier
2007-06-18
Petru Lunca Popa
2007-06-18
Chris Bliss
2007-06-18
Joseph Grogan
Question on PDMS micro channels
Joseph Grogan
2007-06-18
The acetone won't "attack" the PDMS to make it dissolve or anything like
that, but it will strongly affect it by making it swell. Up to you to
determine how much of a problem that causes. I also found the reference
mentioned below to be extremely helpful.
-Joe Grogan

Chris Bliss wrote:
> Hi King,
> The following is a great study investigating solvent compatibility with
> PDMS:
> J. N. Lee, C. Park, and G. M. Whitesides, "Solvent compatibility of
> poly(dimethylsiloxane)-based microfluidic devices," Analytical Chemistry,
> vol. 75, pp. 6544-6554, 2003.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
Mentor Graphics Corporation