HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
2008-05-19
Nataraj
2008-05-19
Brent Garber
2008-05-19
Andrew Sarangan
2008-05-20
Nataraj
2008-05-19
Ravikumar_Kuppan
2008-05-19
walter
Aluminum sputtering and evaporation
2008-05-20
Sreemanth M Uppuluri
2008-05-20
Gary Hillman
2008-05-20
Shay Kaplan
HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
Andrew Sarangan
2008-05-19
Not sure what you mean. Sputtered Aluminum should be a mirror like
surface because it is highly reflective for all visible wavelengths.
If you are not getting a good film I would start by checking the
substrate quality first.


On Mon, May 19, 2008 at 10:40 AM, Brent Garber  wrote:
> Nataraj,
>
> You will need to provide a little more information as how you are depositing
> the aluminum for anyone to help you.
>
> If you are using DC sputtering, I have found the faster the rate the better.
>
> Brent
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.