MEMSnet Home: MEMS-Talk: HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
2008-05-19
Nataraj
2008-05-19
Brent Garber
2008-05-19
Andrew Sarangan
2008-05-20
Nataraj
2008-05-19
Ravikumar_Kuppan
2008-05-19
walter
Aluminum sputtering and evaporation
2008-05-20
Sreemanth M Uppuluri
2008-05-20
Gary Hillman
2008-05-20
Shay Kaplan
HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
Shay Kaplan
2008-05-20
You should start with good surface quality substrate and make sure you base
vacuum is ~10-7 with no water or oxygen.

Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Nataraj
Sent: Monday, May 19, 2008 11:52 AM
To: [email protected]
Subject: [mems-talk] HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING

HAI,

        CAN ANY ONE GIVES IDEAS AS HOW TO IMPROVE THE WHITISH COLOR OF
SPUTTERED ALUMINUM, RIGHT NOW MY SPUTTERED AL COLOR IS SILVER IN COLOR, ANY
SUGGESTION TO IMPROVE THE BRIGHTNESS AND COLOR OF IT ?

Regards,

Nataraj Santhanam
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Nano-Master, Inc.