MEMSnet Home: MEMS-Talk: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
2017-05-01
André Bödecker
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-20
Sangwook Chu
2017-05-01
Orozaliev Ajymurat Nurdinovich
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-01
mercado
2017-05-03
April Maria Lujan
-|EXT|- Re: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-04
MCNIE Mark
2017-05-05
Mehmet Yilmaz
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
Mehmet Yilmaz
2017-04-19
Dear mems-talk community,
I am using "DENKA T-80HW-23A" dicing saw tape to dice MEMS chips from full
4" silicon wafers.

My integration process does not allow me to mechanically peel the diced
tape from the diced MEMS chips. So, I tried acetone to remove the dicing
saw tape (DENKA T-80HW-23A) pieces from the silicon surface of the MEMS
chips. The pieces of dicing tape are removed from the MEMS chips, however,
I realized that, there are very thin layers of residues left on the silicon
surface of the MEMS chips that I cannot remove with acetone.

After drying the MEMS chips with nitrogen blowing, I tried O2 plasma clean
to remove the remaining residues. Most of the residues are gone, but there
are still some residues left that I need to remove.

Could you please let me know how to remove these thin residues of the
dicing saw tape (DENKA T-80HW-23A) from silicon surface?

Thanks in advance,
Sincerely,

Mehmet
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation