MEMSnet Home: MEMS-Talk: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
2017-05-01
André Bödecker
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-20
Sangwook Chu
2017-05-01
Orozaliev Ajymurat Nurdinovich
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-01
mercado
2017-05-03
April Maria Lujan
-|EXT|- Re: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-04
MCNIE Mark
2017-05-05
Mehmet Yilmaz
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
Mehmet Yilmaz
2017-04-19
Dear mems-talk community,
I just wanted to let you know that Piranha cleaning worked fine. Dicing saw
tape residues are completely removed from one of my trial MEMS chips.

I you have some other suggestions that does not require Piranha clean,
please let me know your suggestions. I would be really interested in trying
a residue removal technique that does not require Piranha cleaning.

Thanks in advance,
Sincerely,

Mehmet

On Tue, Mar 21, 2017 at 9:56 PM, Mehmet Yilmaz 
wrote:

> Dear mems-talk community,
> I am using "DENKA T-80HW-23A" dicing saw tape to dice MEMS chips from full
> 4" silicon wafers.
>
> My integration process does not allow me to mechanically peel the diced
> tape from the diced MEMS chips. So, I tried acetone to remove the dicing
> saw tape (DENKA T-80HW-23A) pieces from the silicon surface of the MEMS
> chips. The pieces of dicing tape are removed from the MEMS chips, however,
> I realized that, there are very thin layers of residues left on the silicon
> surface of the MEMS chips that I cannot remove with acetone.
>
> After drying the MEMS chips with nitrogen blowing, I tried O2 plasma clean
> to remove the remaining residues. Most of the residues are gone, but there
> are still some residues left that I need to remove.
>
> Could you please let me know how to remove these thin residues of the
> dicing saw tape (DENKA T-80HW-23A) from silicon surface?
>
> Thanks in advance,
> Sincerely,
>
> Mehmet
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group