MEMSnet Home: MEMS-Talk: Re: Micro-via on glass wafer
Re: Micro-via on glass wafer
1999-03-11
Albert K. Henning
1999-03-11
Robert Okojie
1999-03-11
Shekhar Bhansali
1999-03-11
[email protected]
1999-03-11
Alexander Shenderov
1999-03-11
Hyoung J. Cho
1999-03-11
Erol Harvey
1999-03-15
Roy Knechtel
1999-03-12
Jayant Neogi
Re: Micro-via on glass wafer
Robert Okojie
1999-03-11
Chia-Lun,

Try Accu-Tech Laser Processing.

1175 Linda Vista Drive
San Marcos, CA 92069

(760) 744-6692


On Mar 10, 10:30, Chialun wrote:
> Subject: Micro-via on glass wafer
> This is a multi-part message in MIME format.
>
> ------=_NextPart_000_00B4_01BE6AE0.FC91E170
> Content-Type: text/plain;
>       charset="iso-8859-1"
> Content-Transfer-Encoding: quoted-printable
>
> MEMS Discussion Group,
>  =20
>
>   I am in search of a prototype manufacturing source for drilling =
> micro-vias on glass wafers.  Laser drilling or sand blasting seems like =
> good candidates.  I need holes of diameter of about 150 micrometers on a =
> 7740 glass wafer.  Any help would be greatly appreciated.
>
>
> Chia-Lun Tsai, Ph.D.
>    Research Scientist
>    Integrated Sensing Systems, Inc.
>    387 Airport Industrial Dr.=20
>    Ypsilanti, MI 48198
>    Phone: (734) 547-9896, Ext.115
>    Fax: (734) 547-9964
>    Email: [email protected]
>    http://www.mems-issys.com/
>
>
> ------=_NextPart_000_00B4_01BE6AE0.FC91E170
> Content-Type: text/html;
>       charset="iso-8859-1"
> Content-Transfer-Encoding: quoted-printable
>
> 
> 
> 
>
>  http-equiv=3DContent-Type>
> 
> 
> 
> 
MEMS Discussion Group,
>
 
 
>
  I am in search of a prototype manufacturing = > source for=20 > drilling micro-vias on glass wafers.  L color=3D#000000>aser=20 > drilling or sand blasting seems like good candidates.  I need holes = > of=20 > diameter of about 150 micrometers on a 7740 glass wafer.  Any help = > would be=20 > greatly appreciated.
 
>
 
>
Chia-Lun Tsai, = > Ph.D.
  =20 > Research Scientist
   Integrated Sensing Systems,=20 > Inc.
   387 Airport Industrial Dr.
   = > Ypsilanti, MI=20 > 48198
   Phone: (734) 547-9896, Ext.115
   = > Fax: (734)=20 > 547-9964
   Email: href=3D"mailto:[email protected]">[email protected]
&nbs= > p; =20 > href=3D"http://www.mems-issys.com/">http://www.mems-issys.com/
ONT> 
> > ------=_NextPart_000_00B4_01BE6AE0.FC91E170-- > > >-- End of excerpt from Chialun -- Robert S. Okojie, Ph.D. Senior Engineer Ford Microelectronics 9965 Federal Drive, Colorado Springs, CO 80921-3698 Phone:(719)528-7727; Fax: (719)528-7529 "The frontier of knowledge has no boundary. Paradigms rise and fall"
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation
University Wafer