Re: Micro-via on glass wafer
1999-03-11
Albert K. Henning
1999-03-11
Robert Okojie
1999-03-11
Shekhar Bhansali
1999-03-11
[email protected]
1999-03-11
Alexander Shenderov
1999-03-11
Hyoung J. Cho
1999-03-11
Erol Harvey
1999-03-15
Roy Knechtel
1999-03-12
Jayant Neogi
Re: Micro-via on glass wafer
Alexander Shenderov
1999-03-11
There is an alternative, if you don't care about the sort of glass you
are using - a photoformable glass, called Foturan, from Schott.  It
etches selectively where it has been exposed to light.  Your dimensions
are well within their resolution.

Alex


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review