MEMSnet Home: MEMS-Talk: Re: Piezoelectric materials
Re: Piezoelectric materials
1999-05-12
nigel r. sharma
1999-05-13
Joel Dubow
1999-05-13
Fahrettin Levent Degertekin
Re: Piezoelectric materials
nigel r. sharma
1999-05-12
Try Philips

http://www.passives.comp.philips.com/cgi-bin/hwhsql/sql/naprod.htm?2

Nigel Rudra Sharma
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
email: [email protected]
voice: 206-685-6878
web site: http://lettuce.me.washington.edu/~micropump/
Micropump Research Group
University of Washington, Seattle, USA.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

On Wed, 12 May 1999, F. Sandoval-Ibarra wrote:

> Date: Wed, 12 May 1999 16:57:12 -0500
> From: F. Sandoval-Ibarra 
> Reply-To: [email protected], [email protected],
     [email protected]
> To: [email protected]
> Subject: Piezoelectric materials
>
> Hi!
>
> I am looking for a piezoelectric materials supplier.  I am interested on
> a piezoelectric disk with a diameter of 1-2 cm, 1-5 mm thick, and
> dielectric constant of the order of 1700. In practice, for our
> applications don't care the electrode material.
>
> Can someone please help?
>
> Thanks in advance
>
> Dr. F. Sandoval-Ibarra
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.