Hi.
I suggest you contact EDO Acoustic Products in Salt Lake City. We have used
their material and had good results with it.
regards Joel Dubow
Professor of Materials Science
University of Utah

"F. Sandoval-Ibarra" wrote:

> Hi!
>
> I am looking for a piezoelectric materials supplier.  I am interested on
> a piezoelectric disk with a diameter of 1-2 cm, 1-5 mm thick, and
> dielectric constant of the order of 1700. In practice, for our
> applications don't care the electrode material.
>
> Can someone please help?
>
> Thanks in advance
>
> Dr. F. Sandoval-Ibarra
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing